Chemical properties
Property | Value |
---|---|
Aluminium | 1 % Show Material materials with Aluminium of 1 % |
Andere | total 0.5., Up to 1 % (mass fraction) of the nickel composition can be present as cobalt., Up to 20 % (mass fraction) of the niobium composition can be replaced by tantalum. |
Eisen | 2.5 % Show Material materials with Eisen of 2.5 % |
Kohlenstoff | 0.15 % Show Material materials with Kohlenstoff of 0.15 % |
Kupfer | 28 - 32 % Show Material materials with Kupfer of 28 - 32 % |
Mangan | 4 % Show Material materials with Mangan of 4 % |
Nickel | 60 % Show Material materials with Nickel of 60 % |
Niobium | 3 % Show Material materials with Niobium of 3 % |
Phosphor | 0.02 % Show Material materials with Phosphor of 0.02 % |
Schwefel | 0.015 % Show Material materials with Schwefel of 0.015 % |
Silizium | 1.25 % Show Material materials with Silizium of 1.25 % |
Titan | 1 % Show Material materials with Titan of 1 % |