Chemical properties
Property | Value |
---|---|
Aluminium | 0.75 - 1.2 % Show Material materials with Aluminium of 0.75 - 1.2 % |
Andere | total 0.5., Up to 1 % (mass fraction) of the nickel composition can be present as cobalt., Up to 20 % (mass fraction) of the niobium composition can be replaced by tantalum. |
Bor | 3E-3 % Show Material materials with Bor of 3E-3 % |
Chrom | 36 - 39 % Show Material materials with Chrom of 36 - 39 % |
Eisen | 1 % Show Material materials with Eisen of 1 % |
Kobalt | 1 % Show Material materials with Kobalt of 1 % |
Kohlenstoff | 0.03 % Show Material materials with Kohlenstoff of 0.03 % |
Kupfer | 0.3 % Show Material materials with Kupfer of 0.3 % |
Mangan | 0.5 % Show Material materials with Mangan of 0.5 % |
Molybdän | 0.5 % Show Material materials with Molybdän of 0.5 % |
Nickel | 63 % Show Material materials with Nickel of 63 % |
Niobium | 0.25 - 1 % Show Material materials with Niobium of 0.25 - 1 % |
Phosphor | 0.02 % Show Material materials with Phosphor of 0.02 % |
Schwefel | 0.015 % Show Material materials with Schwefel of 0.015 % |
Silizium | 0.3 % Show Material materials with Silizium of 0.3 % |
Titan | 0.25 - 0.75 % Show Material materials with Titan of 0.25 - 0.75 % |
Zirkonium | 0.02 % Show Material materials with Zirkonium of 0.02 % |