Chemical properties
Property | Value |
---|---|
Andere | total 0.5., Up to 1 % (mass fraction) of the nickel composition can be present as cobalt. |
Chrom | 20.5 - 23 % Show Material materials with Chrom of 20.5 - 23 % |
Eisen | 17 - 20 % Show Material materials with Eisen of 17 - 20 % |
Kobalt | 0.5 - 2.5 % Show Material materials with Kobalt of 0.5 - 2.5 % |
Kohlenstoff | 0.05 - 0.15 % Show Material materials with Kohlenstoff of 0.05 - 0.15 % |
Kupfer | 0.5 % Show Material materials with Kupfer of 0.5 % |
Mangan | 1 % Show Material materials with Mangan of 1 % |
Molybdän | 8 - 10 % Show Material materials with Molybdän of 8 - 10 % |
Nickel | 44 % Show Material materials with Nickel of 44 % |
Phosphor | 0.04 % Show Material materials with Phosphor of 0.04 % |
Schwefel | 0.03 % Show Material materials with Schwefel of 0.03 % |
Silizium | 1 % Show Material materials with Silizium of 1 % |
Wolfram | 0.2 - 1 % Show Material materials with Wolfram of 0.2 - 1 % |