Chemical properties
Property | Value |
---|---|
Aluminium | 1.8 - 2.4 % Show Material materials with Aluminium of 1.8 - 2.4 % |
Andere | total 0.5., Up to 1 % (mass fraction) of the nickel composition can be present as cobalt. |
Chrom | 24 - 26 % Show Material materials with Chrom of 24 - 26 % |
Eisen | 8 - 11 % Show Material materials with Eisen of 8 - 11 % |
Kobalt | 1 % Show Material materials with Kobalt of 1 % |
Kohlenstoff | 0.15 - 0.25 % Show Material materials with Kohlenstoff of 0.15 - 0.25 % |
Kupfer | 0.1 % Show Material materials with Kupfer of 0.1 % |
Mangan | 0.5 % Show Material materials with Mangan of 0.5 % |
Nickel | 59 % Show Material materials with Nickel of 59 % |
Phosphor | 0.02 % Show Material materials with Phosphor of 0.02 % |
Schwefel | 0.015 % Show Material materials with Schwefel of 0.015 % |
Silizium | 0.5 % Show Material materials with Silizium of 0.5 % |
Titan | 0.1 - 0.2 % Show Material materials with Titan of 0.1 - 0.2 % |
Yttrium | 0.05 - 0.12 % Show Material materials with Yttrium of 0.05 - 0.12 % |
Zirkonium | 0.01 - 0.1 % Show Material materials with Zirkonium of 0.01 - 0.1 % |