Chemical properties
Property | Value |
---|---|
Andere | total 0.5., Up to 1 % (mass fraction) of the nickel composition can be present as cobalt., Up to 20 % (mass fraction) of the niobium composition can be replaced by tantalum. |
Chrom | 28 - 31.5 % Show Material materials with Chrom of 28 - 31.5 % |
Eisen | 13 - 17 % Show Material materials with Eisen of 13 - 17 % |
Kobalt | 5 % Show Material materials with Kobalt of 5 % |
Kohlenstoff | 0.03 % Show Material materials with Kohlenstoff of 0.03 % |
Kupfer | 1 - 2.4 % Show Material materials with Kupfer of 1 - 2.4 % |
Mangan | 1.5 % Show Material materials with Mangan of 1.5 % |
Molybdän | 4 - 6 % Show Material materials with Molybdän of 4 - 6 % |
Nickel | 36 % Show Material materials with Nickel of 36 % |
Niobium | 0.3 - 1.5 % Show Material materials with Niobium of 0.3 - 1.5 % |
Phosphor | 0.04 % Show Material materials with Phosphor of 0.04 % |
Schwefel | 0.02 % Show Material materials with Schwefel of 0.02 % |
Silizium | 0.8 % Show Material materials with Silizium of 0.8 % |
Wolfram | 1.5 - 4 % Show Material materials with Wolfram of 1.5 - 4 % |