Chemical properties
Property | Value |
---|---|
Aluminium | 0.3 % Show Material materials with Aluminium of 0.3 % |
Andere | total 0.5., Up to 1 % (mass fraction) of the nickel composition can be present as cobalt. |
Chrom | 26 - 29 % Show Material materials with Chrom of 26 - 29 % |
Eisen | 21 - 25 % Show Material materials with Eisen of 21 - 25 % |
Kobalt | 1 % Show Material materials with Kobalt of 1 % |
Kohlenstoff | 0.05 - 0.12 % Show Material materials with Kohlenstoff of 0.05 - 0.12 % |
Kupfer | 0.3 % Show Material materials with Kupfer of 0.3 % |
Mangan | 1 % Show Material materials with Mangan of 1 % |
Nickel | 40 % Show Material materials with Nickel of 40 % |
Phosphor | 0.02 % Show Material materials with Phosphor of 0.02 % |
Schwefel | 0.01 % Show Material materials with Schwefel of 0.01 % |
Silizium | 2.5 - 3 % Show Material materials with Silizium of 2.5 - 3 % |