Chemical properties
Property | Value |
---|---|
Aluminium | 1.1 % Show Material materials with Aluminium of 1.1 % |
Andere | total 0.5., Al + Ti 1.5. Up to 1 % (mass fraction) of the nickel composition can be present as cobalt., Up to 20 % (mass fraction) of the niobium composition can be replaced by tantalum. |
Chrom | 28 - 31.5 % Show Material materials with Chrom of 28 - 31.5 % |
Eisen | 7 - 11 % Show Material materials with Eisen of 7 - 11 % |
Kohlenstoff | 0.04 % Show Material materials with Kohlenstoff of 0.04 % |
Kupfer | 0.3 % Show Material materials with Kupfer of 0.3 % |
Mangan | 1 % Show Material materials with Mangan of 1 % |
Molybdän | 0.5 % Show Material materials with Molybdän of 0.5 % |
Nickel | 54 % Show Material materials with Nickel of 54 % |
Niobium | 0.1 % Show Material materials with Niobium of 0.1 % |
Phosphor | 0.02 % Show Material materials with Phosphor of 0.02 % |
Schwefel | 0.015 % Show Material materials with Schwefel of 0.015 % |
Silizium | 0.5 % Show Material materials with Silizium of 0.5 % |
Titan | 1 % Show Material materials with Titan of 1 % |