Chemical properties
Property | Value |
---|---|
Aluminium | 1 - 1.7 % Show Material materials with Aluminium of 1 - 1.7 % |
Andere | total 0.5., Up to 1 % (mass fraction) of the nickel composition can be present as cobalt. |
Chrom | 21 - 25 % Show Material materials with Chrom of 21 - 25 % |
Eisen | 20 % Show Material materials with Eisen of 20 % |
Kohlenstoff | 0.1 % Show Material materials with Kohlenstoff of 0.1 % |
Kupfer | 1 % Show Material materials with Kupfer of 1 % |
Mangan | 1 % Show Material materials with Mangan of 1 % |
Nickel | 58 - 63 % Show Material materials with Nickel of 58 - 63 % |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Schwefel | 0.015 % Show Material materials with Schwefel of 0.015 % |
Silizium | 0.5 % Show Material materials with Silizium of 0.5 % |