Chemical properties
Property | Value |
---|---|
Aluminium | 2.5 - 4 % Show Material materials with Aluminium of 2.5 - 4 % |
Andere | total 0.5., Up to 1 % (mass fraction) of the nickel composition can be present as cobalt., Up to 20 % (mass fraction) of the niobium composition can be replaced by tantalum. |
Chrom | 27 - 31 % Show Material materials with Chrom of 27 - 31 % |
Eisen | 2.5 - 6 % Show Material materials with Eisen of 2.5 - 6 % |
Kohlenstoff | 0.15 % Show Material materials with Kohlenstoff of 0.15 % |
Kupfer | 0.5 % Show Material materials with Kupfer of 0.5 % |
Mangan | 1 % Show Material materials with Mangan of 1 % |
Nickel | 53 % Show Material materials with Nickel of 53 % |
Niobium | 0.5 - 2.5 % Show Material materials with Niobium of 0.5 - 2.5 % |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Schwefel | 0.01 % Show Material materials with Schwefel of 0.01 % |
Silizium | 0.5 % Show Material materials with Silizium of 0.5 % |
Titan | 1 % Show Material materials with Titan of 1 % |