Chemical properties
Property | Value |
---|---|
Andere | total 0.5., Up to 1 % (mass fraction) of the nickel composition can be present as cobalt., Up to 20 % (mass fraction) of the niobium composition can be replaced by tantalum. |
Chrom | 33 - 39 % Show Material materials with Chrom of 33 - 39 % |
Eisen | 7 % Show Material materials with Eisen of 7 % |
Kohlenstoff | 0.35 - 0.5 % Show Material materials with Kohlenstoff of 0.35 - 0.5 % |
Mangan | 0.5 - 2 % Show Material materials with Mangan of 0.5 - 2 % |
Nickel | 42 - 48 % Show Material materials with Nickel of 42 - 48 % |
Niobium | 0.8 - 1.8 % Show Material materials with Niobium of 0.8 - 1.8 % |
Phosphor | 0.02 % Show Material materials with Phosphor of 0.02 % |
Schwefel | 0.015 % Show Material materials with Schwefel of 0.015 % |
Silizium | 0.5 - 2 % Show Material materials with Silizium of 0.5 - 2 % |