Chemical properties
Property | Value |
---|---|
Andere | total 0.5., Up to 1 % (mass fraction) of the nickel composition can be present as cobalt. |
Chrom | 23 - 26 % Show Material materials with Chrom of 23 - 26 % |
Eisen | 10 - 17 % Show Material materials with Eisen of 10 - 17 % |
Kohlenstoff | 0.03 % Show Material materials with Kohlenstoff of 0.03 % |
Kupfer | 0.7 - 1.2 % Show Material materials with Kupfer of 0.7 - 1.2 % |
Mangan | 1 % Show Material materials with Mangan of 1 % |
Molybdän | 5 - 7 % Show Material materials with Molybdän of 5 - 7 % |
Nickel | 47 % Show Material materials with Nickel of 47 % |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Schwefel | 0.03 % Show Material materials with Schwefel of 0.03 % |
Silizium | 1 % Show Material materials with Silizium of 1 % |
Titan | 0.7 - 1.5 % Show Material materials with Titan of 0.7 - 1.5 % |