Property | Value |
---|---|
Andere | total 0.5., Up to 1 % (mass fraction) of the nickel composition can be present as cobalt., Up to 20 % (mass fraction) of the niobium composition can be replaced by tantalum. |
Chrom | 21 - 23.5 % Show Material materials with Chrom of 21 - 23.5 % |
Eisen | 18 - 21 % Show Material materials with Eisen of 18 - 21 % |
Kobalt | 5 % Show Material materials with Kobalt of 5 % |
Kohlenstoff | 0.01 % Show Material materials with Kohlenstoff of 0.01 % |
Kupfer | 1.5 - 2.5 % Show Material materials with Kupfer of 1.5 - 2.5 % |
Mangan | 1 % Show Material materials with Mangan of 1 % |
Molybdän | 6 - 8 % Show Material materials with Molybdän of 6 - 8 % |
Nickel | 40 % Show Material materials with Nickel of 40 % |
Niobium | 0.5 % Show Material materials with Niobium of 0.5 % |
Phosphor | 0.04 % Show Material materials with Phosphor of 0.04 % |
Schwefel | 0.03 % Show Material materials with Schwefel of 0.03 % |
Silizium | 1 % Show Material materials with Silizium of 1 % |
Wolfram | 1.5 % Show Material materials with Wolfram of 1.5 % |