Chemical properties
Property | Value |
---|---|
Aluminium | 0.4 - 1 % Show Material materials with Aluminium of 0.4 - 1 % |
Andere | total 0.5., Up to 1 % (mass fraction) of the nickel composition can be present as cobalt., Up to 20 % (mass fraction) of the niobium composition can be replaced by tantalum. |
Chrom | 14 - 17 % Show Material materials with Chrom of 14 - 17 % |
Eisen | 5 - 9 % Show Material materials with Eisen of 5 - 9 % |
Kohlenstoff | 0.08 % Show Material materials with Kohlenstoff of 0.08 % |
Kupfer | 0.5 % Show Material materials with Kupfer of 0.5 % |
Mangan | 1 % Show Material materials with Mangan of 1 % |
Nickel | 70 % Show Material materials with Nickel of 70 % |
Niobium | 0.7 - 1.2 % Show Material materials with Niobium of 0.7 - 1.2 % |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Schwefel | 0.015 % Show Material materials with Schwefel of 0.015 % |
Silizium | 0.5 % Show Material materials with Silizium of 0.5 % |
Titan | 2 - 2.7 % Show Material materials with Titan of 2 - 2.7 % |