Property | Value |
---|---|
Andere | total 0.5., Up to 1 % (mass fraction) of the nickel composition can be present as cobalt. |
Chrom | 14 - 17 % Show Material materials with Chrom of 14 - 17 % |
Eisen | 8 % Show Material materials with Eisen of 8 % |
Kohlenstoff | 0.08 % Show Material materials with Kohlenstoff of 0.08 % |
Kupfer | 0.5 % Show Material materials with Kupfer of 0.5 % |
Mangan | 2 - 2.7 % Show Material materials with Mangan of 2 - 2.7 % |
Nickel | 67 % Show Material materials with Nickel of 67 % |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Schwefel | 0.015 % Show Material materials with Schwefel of 0.015 % |
Silizium | 0.3 % Show Material materials with Silizium of 0.3 % |
Titan | 2.5 - 3.5 % Show Material materials with Titan of 2.5 - 3.5 % |