Chemical properties
Property | Value |
---|---|
Aluminium | 0.2 - 0.8 % Show Material materials with Aluminium of 0.2 - 0.8 % |
Andere | total 0.5., Up to 1 % (mass fraction) of the nickel composition can be present as cobalt., Up to 20 % (mass fraction) of the niobium composition can be replaced by tantalum. |
Bor | 6E-3 % Show Material materials with Bor of 6E-3 % |
Chrom | 17 - 21 % Show Material materials with Chrom of 17 - 21 % |
Eisen | 24 % Show Material materials with Eisen of 24 % |
Kohlenstoff | 0.08 % Show Material materials with Kohlenstoff of 0.08 % |
Kupfer | 0.3 % Show Material materials with Kupfer of 0.3 % |
Mangan | 0.3 % Show Material materials with Mangan of 0.3 % |
Molybdän | 2.8 - 3.3 % Show Material materials with Molybdän of 2.8 - 3.3 % |
Nickel | 50 - 55 % Show Material materials with Nickel of 50 - 55 % |
Niobium | 4.8 - 5.5 % Show Material materials with Niobium of 4.8 - 5.5 % |
Phosphor | 0.02 % Show Material materials with Phosphor of 0.02 % |
Schwefel | 0.015 % Show Material materials with Schwefel of 0.015 % |
Silizium | 0.3 % Show Material materials with Silizium of 0.3 % |
Titan | 0.7 - 1.1 % Show Material materials with Titan of 0.7 - 1.1 % |