Chemical properties
Property | Value |
---|---|
Andere | total 0.5., Up to 1 % (mass fraction) of the nickel composition can be present as cobalt. |
Chrom | 1 % Show Material materials with Chrom of 1 % |
Eisen | 4 - 7 % Show Material materials with Eisen of 4 - 7 % |
Kobalt | 2.5 % Show Material materials with Kobalt of 2.5 % |
Kohlenstoff | 0.08 % Show Material materials with Kohlenstoff of 0.08 % |
Kupfer | 0.5 % Show Material materials with Kupfer of 0.5 % |
Mangan | 1 % Show Material materials with Mangan of 1 % |
Molybdän | 26 - 30 % Show Material materials with Molybdän of 26 - 30 % |
Nickel | 55 % Show Material materials with Nickel of 55 % |
Phosphor | 0.02 % Show Material materials with Phosphor of 0.02 % |
Schwefel | 0.03 % Show Material materials with Schwefel of 0.03 % |
Silizium | 1 % Show Material materials with Silizium of 1 % |
Vanadium | 0.2 - 0.4 % Show Material materials with Vanadium of 0.2 - 0.4 % |
Wolfram | 1 % Show Material materials with Wolfram of 1 % |