Chemical properties
Property | Value |
---|---|
Andere | total 0.5., Up to 1 % (mass fraction) of the nickel composition can be present as cobalt. |
Chrom | 4 - 6 % Show Material materials with Chrom of 4 - 6 % |
Eisen | 4 - 7 % Show Material materials with Eisen of 4 - 7 % |
Kobalt | 2.5 % Show Material materials with Kobalt of 2.5 % |
Kohlenstoff | 0.12 % Show Material materials with Kohlenstoff of 0.12 % |
Kupfer | 0.5 % Show Material materials with Kupfer of 0.5 % |
Mangan | 1 % Show Material materials with Mangan of 1 % |
Molybdän | 23 - 26 % Show Material materials with Molybdän of 23 - 26 % |
Nickel | 62 % Show Material materials with Nickel of 62 % |
Phosphor | 0.04 % Show Material materials with Phosphor of 0.04 % |
Schwefel | 0.03 % Show Material materials with Schwefel of 0.03 % |
Silizium | 1 % Show Material materials with Silizium of 1 % |
Vanadium | 0.6 % Show Material materials with Vanadium of 0.6 % |
Wolfram | 1 % Show Material materials with Wolfram of 1 % |