Chemical properties
Property | Value |
---|---|
Andere | total 0.5., Up to 1 % (mass fraction) of the nickel composition can be present as cobalt. |
Chrom | 0.5 - 3.5 % Show Material materials with Chrom of 0.5 - 3.5 % |
Eisen | 10 % Show Material materials with Eisen of 10 % |
Kohlenstoff | 0.1 % Show Material materials with Kohlenstoff of 0.1 % |
Kupfer | 0.5 % Show Material materials with Kupfer of 0.5 % |
Mangan | 1 % Show Material materials with Mangan of 1 % |
Molybdän | 18 - 21 % Show Material materials with Molybdän of 18 - 21 % |
Nickel | 60 % Show Material materials with Nickel of 60 % |
Phosphor | 0.02 % Show Material materials with Phosphor of 0.02 % |
Schwefel | 0.015 % Show Material materials with Schwefel of 0.015 % |
Silizium | 0.5 % Show Material materials with Silizium of 0.5 % |
Wolfram | 2 - 4 % Show Material materials with Wolfram of 2 - 4 % |