Chemical properties
Property | Value |
---|---|
Aluminium | 0.5 % Show Material materials with Aluminium of 0.5 % |
Andere | total 0.5., Up to 1 % (mass fraction) of the nickel composition can be present as cobalt. |
Chrom | 7 - 9 % Show Material materials with Chrom of 7 - 9 % |
Eisen | 2 % Show Material materials with Eisen of 2 % |
Kobalt | 1 % Show Material materials with Kobalt of 1 % |
Kohlenstoff | 0.03 % Show Material materials with Kohlenstoff of 0.03 % |
Kupfer | 0.5 % Show Material materials with Kupfer of 0.5 % |
Mangan | 0.8 % Show Material materials with Mangan of 0.8 % |
Molybdän | 24 - 26 % Show Material materials with Molybdän of 24 - 26 % |
Nickel | 59 % Show Material materials with Nickel of 59 % |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Schwefel | 0.015 % Show Material materials with Schwefel of 0.015 % |
Silizium | 0.8 % Show Material materials with Silizium of 0.8 % |