Chemical properties
Property | Value |
---|---|
Andere | total 0.5., Up to 1 % (mass fraction) of the nickel composition can be present as cobalt. |
Chrom | 1 % Show Material materials with Chrom of 1 % |
Eisen | 2 % Show Material materials with Eisen of 2 % |
Kobalt | 1 % Show Material materials with Kobalt of 1 % |
Kohlenstoff | 0.02 % Show Material materials with Kohlenstoff of 0.02 % |
Kupfer | 0.5 % Show Material materials with Kupfer of 0.5 % |
Mangan | 1 % Show Material materials with Mangan of 1 % |
Molybdän | 26 - 30 % Show Material materials with Molybdän of 26 - 30 % |
Nickel | 64 % Show Material materials with Nickel of 64 % |
Phosphor | 0.04 % Show Material materials with Phosphor of 0.04 % |
Schwefel | 0.03 % Show Material materials with Schwefel of 0.03 % |
Silizium | 0.1 % Show Material materials with Silizium of 0.1 % |
Titan | 0.5 % Show Material materials with Titan of 0.5 % |
Wolfram | 1 % Show Material materials with Wolfram of 1 % |