Chemical properties
Property | Value |
---|---|
Andere | total 0.5., Up to 1 % (mass fraction) of the nickel composition can be present as cobalt. |
Chrom | 20 - 22.5 % Show Material materials with Chrom of 20 - 22.5 % |
Eisen | 2 - 6 % Show Material materials with Eisen of 2 - 6 % |
Kobalt | 2.5 % Show Material materials with Kobalt of 2.5 % |
Kohlenstoff | 0.01 % Show Material materials with Kohlenstoff of 0.01 % |
Kupfer | 0.5 % Show Material materials with Kupfer of 0.5 % |
Mangan | 0.5 % Show Material materials with Mangan of 0.5 % |
Molybdän | 12.5 - 14.5 % Show Material materials with Molybdän of 12.5 - 14.5 % |
Nickel | 49 % Show Material materials with Nickel of 49 % |
Phosphor | 0.02 % Show Material materials with Phosphor of 0.02 % |
Schwefel | 0.015 % Show Material materials with Schwefel of 0.015 % |
Silizium | 0.08 % Show Material materials with Silizium of 0.08 % |
Vanadium | 0.3 % Show Material materials with Vanadium of 0.3 % |
Wolfram | 2.5 - 3.5 % Show Material materials with Wolfram of 2.5 - 3.5 % |