Chemical properties
Property | Value |
---|---|
Aluminium | 0.05 - 0.5 % Show Material materials with Aluminium of 0.05 - 0.5 % |
Andere | total 0.5., Up to 1 % (mass fraction) of the nickel composition can be present as cobalt., Up to 20 % (mass fraction) of the niobium composition can be replaced by tantalum. |
Chrom | 19 - 21 % Show Material materials with Chrom of 19 - 21 % |
Eisen | 12 - 16 % Show Material materials with Eisen of 12 - 16 % |
Kobalt | 1 % Show Material materials with Kobalt of 1 % |
Kohlenstoff | 0.03 % Show Material materials with Kohlenstoff of 0.03 % |
Kupfer | 0.3 % Show Material materials with Kupfer of 0.3 % |
Mangan | 0.5 % Show Material materials with Mangan of 0.5 % |
Molybdän | 9.5 - 12.5 % Show Material materials with Molybdän of 9.5 - 12.5 % |
Nickel | 44 % Show Material materials with Nickel of 44 % |
Niobium | 0.05 - 0.5 % Show Material materials with Niobium of 0.05 - 0.5 % |
Phosphor | 0.02 % Show Material materials with Phosphor of 0.02 % |
Schwefel | 0.01 % Show Material materials with Schwefel of 0.01 % |
Silizium | 0.5 % Show Material materials with Silizium of 0.5 % |
Stickstoff | 0.05 - 0.2 % Show Material materials with Stickstoff of 0.05 - 0.2 % |
Vanadium | 0.3 % Show Material materials with Vanadium of 0.3 % |
Wolfram | 0.5 - 2.5 % Show Material materials with Wolfram of 0.5 - 2.5 % |