Chemical properties
Property | Value |
---|---|
Aluminium | 0.5 % Show Material materials with Aluminium of 0.5 % |
Andere | total 0.5., Up to 1 % (mass fraction) of the nickel composition can be present as cobalt. |
Chrom | 19 - 23 % Show Material materials with Chrom of 19 - 23 % |
Eisen | 5 % Show Material materials with Eisen of 5 % |
Kohlenstoff | 0.01 % Show Material materials with Kohlenstoff of 0.01 % |
Kupfer | 0.5 % Show Material materials with Kupfer of 0.5 % |
Mangan | 1 % Show Material materials with Mangan of 1 % |
Molybdän | 15 - 17 % Show Material materials with Molybdän of 15 - 17 % |
Nickel | 49 % Show Material materials with Nickel of 49 % |
Phosphor | 0.02 % Show Material materials with Phosphor of 0.02 % |
Schwefel | 0.02 % Show Material materials with Schwefel of 0.02 % |
Silizium | 0.08 % Show Material materials with Silizium of 0.08 % |
Titan | 0.25 % Show Material materials with Titan of 0.25 % |
Wolfram | 3 - 4.4 % Show Material materials with Wolfram of 3 - 4.4 % |