Chemical properties
Property | Value |
---|---|
Aluminium | 0.4 % Show Material materials with Aluminium of 0.4 % |
Andere | total 0.5., Up to 1 % (mass fraction) of the nickel composition can be present as cobalt., Up to 20 % (mass fraction) of the niobium composition can be replaced by tantalum. |
Chrom | 26 - 29 % Show Material materials with Chrom of 26 - 29 % |
Eisen | 3.5 % Show Material materials with Eisen of 3.5 % |
Kobalt | 27 - 32 % Show Material materials with Kobalt of 27 - 32 % |
Kohlenstoff | 0.02 - 0.1 % Show Material materials with Kohlenstoff of 0.02 - 0.1 % |
Kupfer | 0.5 % Show Material materials with Kupfer of 0.5 % |
Mangan | 1 % Show Material materials with Mangan of 1 % |
Molybdän | 0.7 % Show Material materials with Molybdän of 0.7 % |
Nickel | 30 % Show Material materials with Nickel of 30 % |
Niobium | 0.3 % Show Material materials with Niobium of 0.3 % |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Schwefel | 0.015 % Show Material materials with Schwefel of 0.015 % |
Silizium | 2.4 - 3 % Show Material materials with Silizium of 2.4 - 3 % |
Titan | 0.2 - 0.6 % Show Material materials with Titan of 0.2 - 0.6 % |
Wolfram | 0.5 % Show Material materials with Wolfram of 0.5 % |