Chemical properties
Property | Value |
---|---|
Aluminium | 1 - 2 % Show Material materials with Aluminium of 1 - 2 % |
Andere | total 0.5., Up to 1 % (mass fraction) of the nickel composition can be present as cobalt. |
Bismut | 1E-4 % Show Material materials with Bismut of 1E-4 % |
Blei | 2E-3 % Show Material materials with Blei of 2E-3 % |
Bor | 0.02 % Show Material materials with Bor of 0.02 % |
Chrom | 18 - 21 % Show Material materials with Chrom of 18 - 21 % |
Eisen | 1.5 % Show Material materials with Eisen of 1.5 % |
Kobalt | 15 - 18 % Show Material materials with Kobalt of 15 - 18 % |
Kohlenstoff | 0.13 % Show Material materials with Kohlenstoff of 0.13 % |
Kupfer | 0.2 % Show Material materials with Kupfer of 0.2 % |
Mangan | 1 % Show Material materials with Mangan of 1 % |
Nickel | 50 % Show Material materials with Nickel of 50 % |
Phosphor | 0.02 % Show Material materials with Phosphor of 0.02 % |
Schwefel | 0.015 % Show Material materials with Schwefel of 0.015 % |
Silber | 5E-4 % Show Material materials with Silber of 5E-4 % |
Silizium | 1 % Show Material materials with Silizium of 1 % |
Titan | 2 - 3 % Show Material materials with Titan of 2 - 3 % |
Zirkonium | 0.15 % Show Material materials with Zirkonium of 0.15 % |