Chemical properties
Property | Value |
---|---|
Aluminium | 0.3 - 0.6 % Show Material materials with Aluminium of 0.3 - 0.6 % |
Andere | total 0.5., Al + Ti 2.4 - 2.8. Up to 1 % (mass fraction) of the nickel composition can be present as cobalt. |
Bismut | 1E-4 % Show Material materials with Bismut of 1E-4 % |
Bor | 5E-3 % Show Material materials with Bor of 5E-3 % |
Chrom | 19 - 21 % Show Material materials with Chrom of 19 - 21 % |
Eisen | 0.7 % Show Material materials with Eisen of 0.7 % |
Kobalt | 19 - 21 % Show Material materials with Kobalt of 19 - 21 % |
Kohlenstoff | 0.04 - 0.08 % Show Material materials with Kohlenstoff of 0.04 - 0.08 % |
Kupfer | 0.2 % Show Material materials with Kupfer of 0.2 % |
Mangan | 0.6 % Show Material materials with Mangan of 0.6 % |
Molybdän | 5.6 - 6.1 % Show Material materials with Molybdän of 5.6 - 6.1 % |
Nickel | 47 % Show Material materials with Nickel of 47 % |
Phosphor | 0.02 % Show Material materials with Phosphor of 0.02 % |
Schwefel | 7E-3 % Show Material materials with Schwefel of 7E-3 % |
Silber | 5E-4 % Show Material materials with Silber of 5E-4 % |
Silizium | 0.4 % Show Material materials with Silizium of 0.4 % |
Titan | 1.9 - 2.4 % Show Material materials with Titan of 1.9 - 2.4 % |