Chemical properties
Property | Value |
---|---|
Aluminium | 0.2 - 0.5 % Show Material materials with Aluminium of 0.2 - 0.5 % |
Andere | total 0.5., Up to 1 % (mass fraction) of the nickel composition can be present as cobalt. |
Chrom | 20 - 24 % Show Material materials with Chrom of 20 - 24 % |
Eisen | 3 % Show Material materials with Eisen of 3 % |
Kobalt | 5 % Show Material materials with Kobalt of 5 % |
Kohlenstoff | 0.05 - 0.15 % Show Material materials with Kohlenstoff of 0.05 - 0.15 % |
Kupfer | 0.5 % Show Material materials with Kupfer of 0.5 % |
Mangan | 0.3 - 1 % Show Material materials with Mangan of 0.3 - 1 % |
Molybdän | 1 - 3 % Show Material materials with Molybdän of 1 - 3 % |
Nickel | 48 % Show Material materials with Nickel of 48 % |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Schwefel | 0.015 % Show Material materials with Schwefel of 0.015 % |
Silizium | 0.25 - 0.75 % Show Material materials with Silizium of 0.25 - 0.75 % |
Wolfram | 13 - 15 % Show Material materials with Wolfram of 13 - 15 % |