Chemical properties
Property | Value |
---|---|
Aluminium | 0.5 % Show Material materials with Aluminium of 0.5 % |
Andere | total 0.5.ausgenommen Co and Ta, Up to 1 % (mass fraction) of the nickel composition can be present as cobalt., Up to 20 % (mass fraction) of the niobium composition can be replaced by tantalum. |
Chrom | 28 - 31.5 % Show Material materials with Chrom of 28 - 31.5 % |
Eisen | 7 - 12 % Show Material materials with Eisen of 7 - 12 % |
Kohlenstoff | 0.05 % Show Material materials with Kohlenstoff of 0.05 % |
Kupfer | 0.5 % Show Material materials with Kupfer of 0.5 % |
Mangan | 5 % Show Material materials with Mangan of 5 % |
Molybdän | 0.5 % Show Material materials with Molybdän of 0.5 % |
Nickel | 50 % Show Material materials with Nickel of 50 % |
Niobium | 1 - 2.5 % Show Material materials with Niobium of 1 - 2.5 % |
Phosphor | 0.02 % Show Material materials with Phosphor of 0.02 % |
Schwefel | 0.015 % Show Material materials with Schwefel of 0.015 % |
Silizium | 0.8 % Show Material materials with Silizium of 0.8 % |
Titan | 0.5 % Show Material materials with Titan of 0.5 % |