Chemical properties
Property | Value |
---|---|
Andere | total 0.5.ausgenommen Co and Ta, Up to 1 % (mass fraction) of the nickel composition can be present as cobalt. |
Chrom | 24 - 26 % Show Material materials with Chrom of 24 - 26 % |
Eisen | 16 % Show Material materials with Eisen of 16 % |
Kobalt | 2.5 - 3.5 % Show Material materials with Kobalt of 2.5 - 3.5 % |
Kohlenstoff | 0.1 % Show Material materials with Kohlenstoff of 0.1 % |
Kupfer | 0.5 % Show Material materials with Kupfer of 0.5 % |
Mangan | 1.2 - 2 % Show Material materials with Mangan of 1.2 - 2 % |
Molybdän | 2.5 - 3.5 % Show Material materials with Molybdän of 2.5 - 3.5 % |
Nickel | 44 - 47 % Show Material materials with Nickel of 44 - 47 % |
Phosphor | 0.02 % Show Material materials with Phosphor of 0.02 % |
Schwefel | 0.015 % Show Material materials with Schwefel of 0.015 % |
Silizium | 0.8 - 1.2 % Show Material materials with Silizium of 0.8 - 1.2 % |
Wolfram | 2.5 - 3.5 % Show Material materials with Wolfram of 2.5 - 3.5 % |