Chemical properties
Property | Value |
---|---|
Andere | total 0.5.ausgenommen Co and Ta, Up to 1 % (mass fraction) of the nickel composition can be present as cobalt. |
Chrom | 27 - 30 % Show Material materials with Chrom of 27 - 30 % |
Eisen | 6 % Show Material materials with Eisen of 6 % |
Kohlenstoff | 0.35 - 0.5 % Show Material materials with Kohlenstoff of 0.35 - 0.5 % |
Mangan | 0.5 - 1.5 % Show Material materials with Mangan of 0.5 - 1.5 % |
Nickel | 47 - 50 % Show Material materials with Nickel of 47 - 50 % |
Phosphor | 0.02 % Show Material materials with Phosphor of 0.02 % |
Schwefel | 0.015 % Show Material materials with Schwefel of 0.015 % |
Silizium | 0.5 - 2 % Show Material materials with Silizium of 0.5 - 2 % |