Chemical properties
Property | Value |
---|---|
Aluminium | 0.1 % Show Material materials with Aluminium of 0.1 % |
Andere | total 0.5.ausgenommen Co and Ta, Up to 1 % (mass fraction) of the nickel composition can be present as cobalt. |
Chrom | 23 - 27 % Show Material materials with Chrom of 23 - 27 % |
Eisen | 30 % Show Material materials with Eisen of 30 % |
Kohlenstoff | 0.03 % Show Material materials with Kohlenstoff of 0.03 % |
Kupfer | 1.5 - 3 % Show Material materials with Kupfer of 1.5 - 3 % |
Mangan | 1 - 3 % Show Material materials with Mangan of 1 - 3 % |
Molybdän | 3.5 - 7.5 % Show Material materials with Molybdän of 3.5 - 7.5 % |
Nickel | 37 - 42 % Show Material materials with Nickel of 37 - 42 % |
Phosphor | 0.02 % Show Material materials with Phosphor of 0.02 % |
Schwefel | 0.015 % Show Material materials with Schwefel of 0.015 % |
Silizium | 0.7 % Show Material materials with Silizium of 0.7 % |
Titan | 1 % Show Material materials with Titan of 1 % |