Chemical properties
Property | Value |
---|---|
Andere | total 0.5.ausgenommen Co and Ta, Up to 1 % (mass fraction) of the nickel composition can be present as cobalt. |
Chrom | 25 - 27 % Show Material materials with Chrom of 25 - 27 % |
Eisen | 1.5 % Show Material materials with Eisen of 1.5 % |
Kohlenstoff | 0.02 % Show Material materials with Kohlenstoff of 0.02 % |
Kupfer | 0.5 % Show Material materials with Kupfer of 0.5 % |
Mangan | 0.5 % Show Material materials with Mangan of 0.5 % |
Molybdän | 13.5 - 15 % Show Material materials with Molybdän of 13.5 - 15 % |
Nickel | 55 % Show Material materials with Nickel of 55 % |
Phosphor | 0.02 % Show Material materials with Phosphor of 0.02 % |
Schwefel | 0.015 % Show Material materials with Schwefel of 0.015 % |
Silizium | 0.2 % Show Material materials with Silizium of 0.2 % |