Chemical properties
Property | Value |
---|---|
Andere | total 0.5.ausgenommen Co and Ta, Up to 1 % (mass fraction) of the nickel composition can be present as cobalt. |
Chrom | 14.5 - 16.5 % Show Material materials with Chrom of 14.5 - 16.5 % |
Eisen | 4 - 7 % Show Material materials with Eisen of 4 - 7 % |
Kobalt | 2.5 % Show Material materials with Kobalt of 2.5 % |
Kohlenstoff | 0.1 % Show Material materials with Kohlenstoff of 0.1 % |
Kupfer | 0.5 % Show Material materials with Kupfer of 0.5 % |
Mangan | 1 % Show Material materials with Mangan of 1 % |
Molybdän | 15 - 18 % Show Material materials with Molybdän of 15 - 18 % |
Nickel | 50 % Show Material materials with Nickel of 50 % |
Phosphor | 0.02 % Show Material materials with Phosphor of 0.02 % |
Schwefel | 0.015 % Show Material materials with Schwefel of 0.015 % |
Silizium | 1 % Show Material materials with Silizium of 1 % |
Vanadium | 0.4 % Show Material materials with Vanadium of 0.4 % |
Wolfram | 3 - 4.5 % Show Material materials with Wolfram of 3 - 4.5 % |