Chemical properties
Property | Value |
---|---|
Andere | total 0.5.ausgenommen Co and Ta, Up to 1 % (mass fraction) of the nickel composition can be present as cobalt., Up to 20 % (mass fraction) of the niobium composition can be replaced by tantalum. |
Chrom | 12 - 17 % Show Material materials with Chrom of 12 - 17 % |
Eisen | 10 % Show Material materials with Eisen of 10 % |
Kohlenstoff | 0.1 % Show Material materials with Kohlenstoff of 0.1 % |
Kupfer | 0.5 % Show Material materials with Kupfer of 0.5 % |
Mangan | 2 - 4 % Show Material materials with Mangan of 2 - 4 % |
Molybdän | 5 - 9 % Show Material materials with Molybdän of 5 - 9 % |
Nickel | 55 % Show Material materials with Nickel of 55 % |
Niobium | 0.5 - 2 % Show Material materials with Niobium of 0.5 - 2 % |
Phosphor | 0.02 % Show Material materials with Phosphor of 0.02 % |
Schwefel | 0.015 % Show Material materials with Schwefel of 0.015 % |
Silizium | 1 % Show Material materials with Silizium of 1 % |
Wolfram | 1 - 2 % Show Material materials with Wolfram of 1 - 2 % |