Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 8.1 g/cm³ Show Material materials with Dichte of 8.1 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 23.0 °C | 50 GPa Show Material materials with Elastizitätsmodul of 50 GPa | Typical for Cadmium |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Cadmium |
Schubmodule | 23.0 °C | 19.2 GPa Show Material materials with Schubmodule of 19.2 GPa | Typical for Cadmium |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 3E-5 - 3.2E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 3E-5 - 3.2E-5 1/K | Typical for Cadmium |
Schmelzpunkt | 265 - 280 °C Show Material materials with Schmelzpunkt of 265 - 280 °C | ||
Spezifische Wärmekapazität | 23.0 °C | 230 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 230 J/(kg·K) | Typical for Cadmium |
Wärmeleitfähigkeit | 23.0 °C | 84 - 97 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 84 - 97 W/(m·K) | Typical for Cadmium |
Chemical properties
Property | Value |
---|---|
Aluminium | 1E-3 % Show Material materials with Aluminium of 1E-3 % |
Andere | Rest Cd |
Antimon | 0.1 % Show Material materials with Antimon of 0.1 % |
Arsen | 0.03 % Show Material materials with Arsen of 0.03 % |
Bismut | 0.1 % Show Material materials with Bismut of 0.1 % |
Blei | 0.1 % Show Material materials with Blei of 0.1 % |
Eisen | 0.02 % Show Material materials with Eisen of 0.02 % |
Gold | 0.05 % Show Material materials with Gold of 0.05 % |
Indium | 0.1 % Show Material materials with Indium of 0.1 % |
Kupfer | 0.1 % Show Material materials with Kupfer of 0.1 % |
Nickel | 0.01 % Show Material materials with Nickel of 0.01 % |
Silber | 0.1 % Show Material materials with Silber of 0.1 % |
Zink | 17 - 25 % Show Material materials with Zink of 17 - 25 % |
Zinn | 0.1 % Show Material materials with Zinn of 0.1 % |