Allgemein
Property | Value | Condition | Related Standards |
---|---|---|---|
Dichte | 2.65 g/cm³ Show Material materials with Dichte of 2.65 g/cm³ | F | EN 1706 |
Mechanisch
Property | Value | Condition | Related Standards | Comment |
---|---|---|---|---|
Bending Fatigue Strength | 80.0 - 110.0 MPa Show Material materials with Bending Fatigue Strength of 80.0 - 110.0 MPa | F | EN 1706 | |
Elastizitätsmodul | 74.0 GPa Show Material materials with Elastizitätsmodul of 74.0 GPa | F | EN 1706 | |
Härte, Brinell | 50.0 [-] Show Material materials with Härte, Brinell of 50.0 [-] | F | EN 1706 | |
55.0 [-] Show Material materials with Härte, Brinell of 55.0 [-] | F | EN 1706 | ||
Poissonzahl | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | Typical for Cast 3xx.x Series Aluminium | ||
Schubmodule | 2.8 GPa Show Material materials with Schubmodule of 2.8 GPa | Typical for Cast 3xx.x Series Aluminium | ||
Zugfestigkeit | 160.0 MPa Show Material materials with Zugfestigkeit of 160.0 MPa | F | EN 1706 | |
180.0 MPa Show Material materials with Zugfestigkeit of 180.0 MPa | F | EN 1706 |
Thermisch
Property | Temperature | Value | Condition | Related Standards |
---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 20 °C | 2.1e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.1e-05 1/K | F | EN 1706 |
100 °C | 2.1e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.1e-05 1/K | F | EN 1706 | |
Schmelzpunkt | 530.0 - 600.0 °C Show Material materials with Schmelzpunkt of 530.0 - 600.0 °C | F | EN 1706 | |
Spezifische Wärmekapazität | 900.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 900.0 J/(kg·K) | F | EN 1706 | |
Wärmeleitfähigkeit | 130.0 - 170.0 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 130.0 - 170.0 W/(m·K) | F | EN 1706 |
Elektrisch
Property | Value | Condition | Related Standards |
---|---|---|---|
Elektrische Leitfähigkeit | 16000000.0 - 24000000.0 S/m Show Material materials with Elektrische Leitfähigkeit of 16000000.0 - 24000000.0 S/m | F | EN 1706 |
spezifischer Widerstand | 4.17e-08 - 6.25e-08 Ω·m Show Material materials with spezifischer Widerstand of 4.17e-08 - 6.25e-08 Ω·m | F | EN 1706 |
Chemical properties
Property | Value | Condition | Related Standards |
---|---|---|---|
Eisen | 1.00 % Show Material materials with Eisen of 1.00 % | F | EN 1706 |
Kupfer | 0.1 % Show Material materials with Kupfer of 0.1 % | F | EN 1706 |
Magnesium | 0.5 % Show Material materials with Magnesium of 0.5 % | F | EN 1706 |
Mangan | 0.001 - 0.4 % Show Material materials with Mangan of 0.001 - 0.4 % | F | EN 1706 |
Silizium | 9.0 - 11.0 % Show Material materials with Silizium of 9.0 - 11.0 % | F | EN 1706 |
Titan | 0.15 % Show Material materials with Titan of 0.15 % | F | EN 1706 |
Zink | 0.1 % Show Material materials with Zink of 0.1 % | F | EN 1706 |
Technological properties
Property | ||
---|---|---|
Anodizing | decorative: not recommended | |
Corrosion properties | general: acceptable | |
General machinability | after thermal treatment: good to acceptable, as cast: good |