Allgemein
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Dichte | 2.71 g/cm³ Show Material materials with Dichte of 2.71 g/cm³ | H22 | EN 573-3, EN 485, EN 541, EN 546, EN 683 | ||
20.0 °C | 2.71 g/cm³ Show Material materials with Dichte of 2.71 g/cm³ | H22 | DIN 1725-1, EN 573-3, EN 573-4 | Flat |
Mechanisch
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Elastizitätsmodul | 70.0 GPa Show Material materials with Elastizitätsmodul of 70.0 GPa | H22 | EN 573-3, EN 485, EN 541, EN 546, EN 683 | |||
Härte, Brinell | 35.0 [-] Show Material materials with Härte, Brinell of 35.0 [-] | H22 | EN 573-3, EN 485 | |||
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 8000 Series Aluminium | ||||
Poissonzahl | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | Typical for Wrought 8000 Series Aluminium | ||||
Zugfestigkeit | 90.0 - 150.0 MPa Show Material materials with Zugfestigkeit of 90.0 - 150.0 MPa | H22 | EN 573-3, EN 546, EN 683 | |||
105.0 - 145.0 MPa Show Material materials with Zugfestigkeit of 105.0 - 145.0 MPa | H22 | EN 573-3, EN 485, EN 541 | ||||
20.0 °C | 110.0 - 150.0 MPa Show Material materials with Zugfestigkeit of 110.0 - 150.0 MPa | H22 | DIN 1725-1, EN 573-3, EN 573-4 | Flat |
Thermisch
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 20 °C | 2.35e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.35e-05 1/K | H22 | EN 573-3, EN 485, EN 541, EN 546, EN 683 | ||
100 °C | 2.35e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.35e-05 1/K | H22 | EN 573-3, EN 485, EN 541, EN 546, EN 683 | |||
Schmelzpunkt | 640.0 - 655.0 °C Show Material materials with Schmelzpunkt of 640.0 - 655.0 °C | H22 | EN 573-3, EN 485, EN 541, EN 546, EN 683 | |||
Spezifische Wärmekapazität | 920.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 920.0 J/(kg·K) | Typical for Wrought 8000 Series Aluminium | ||||
Wärmeleitfähigkeit | 20.0 °C | 210.0 - 220.0 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 210.0 - 220.0 W/(m·K) | H22 | DIN 1725-1, EN 573-3, EN 573-4, EN 485, EN 541, EN 546, EN 683 | Flat |
Elektrisch
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Elektrische Leitfähigkeit | 20.0 °C | 34000000.0 - 35000000.0 S/m Show Material materials with Elektrische Leitfähigkeit of 34000000.0 - 35000000.0 S/m | H22 | DIN 1725-1, EN 573-3, EN 573-4, EN 485, EN 541, EN 546, EN 683 | Flat |
spezifischer Widerstand | 2.86e-08 - 2.94e-08 Ω·m Show Material materials with spezifischer Widerstand of 2.86e-08 - 2.94e-08 Ω·m | H22 | EN 573-3, EN 485, EN 541, EN 546, EN 683 |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Chrom | 0.1 % Show Material materials with Chrom of 0.1 % | H22 | EN 573-3, EN 485, EN 541, EN 546, EN 683 | |
Eisen | 0.5 - 1.0 % Show Material materials with Eisen of 0.5 - 1.0 % | H22 | DIN 1725-1, EN 573-3, EN 573-4, EN 485, EN 541, EN 546, EN 683 | Flat |
Kupfer | 0.1 % Show Material materials with Kupfer of 0.1 % | H22 | DIN 1725-1, EN 573-3, EN 573-4, EN 485, EN 541, EN 546, EN 683 | Flat |
Magnesium | 0.1 % Show Material materials with Magnesium of 0.1 % | H22 | EN 573-3, EN 485, EN 541, EN 546, EN 683 | |
Mangan | 0.1 % Show Material materials with Mangan of 0.1 % | H22 | DIN 1725-1, EN 573-3, EN 573-4, EN 485, EN 541, EN 546, EN 683 | Flat |
Silizium | 0.4 - 0.8 % Show Material materials with Silizium of 0.4 - 0.8 % | H22 | DIN 1725-1, EN 573-3, EN 573-4, EN 485, EN 541, EN 546, EN 683 | Flat |
Titan | 0.05 Show Material materials with Titan of 0.05 | H22 | DIN 1725-1, EN 573-3, EN 573-4 | Flat |
Zink | 0.1 % Show Material materials with Zink of 0.1 % | H22 | DIN 1725-1, EN 573-3, EN 573-4, EN 485, EN 541, EN 546, EN 683 | Flat |