DIN 1725-1 Grade 3.0915 H24

Want to keep this datasheet? Save it now in your required format

Description

The alloy AlFeSi is alloyed for increasing the strength increase with Fe and Si. The material belongs to the nature-hard aluminum materials. A strength increase can be achieved only by cold forming. The alloy AlFeSi is very well cold and warm formable and has a good thermal and relatively good electrical conductivity. The material is particularly suitable for deep-drawing. It is well solderable. The material is to be oxidized well anodically, i.e. a shining clean surface develops. It is standardised as sheet metal or strip (DIN 1788 and DIN 1745). Application: for screw-type caps, for menu bowls, for light containers, bottle caps, cover containers and other form packing, for metal goods, like trim, decorated tiles, flexible pipes, various deep-drawing products, for heat exchangers and radiator fins

Related Standards

Equivalent Materials

Diese Materialdaten wurden von WIAM,AluKey zur Verfügung gestellt

Alle Daten beziehen sich auf Raumtemperatur soweit nicht anderweitig spezifiziert. SI Einheiten werden verwendt soweit nicht anderweitig spezifiziert.
Äquivalente Standards sind ähnlich zu einem oder mehreren Standards die der Anbieter angegeben hat. Manche äquivalente Standards können strikter sein oder außerhalb der Bedingungen des ursprünglichen Standards.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Eigenschaften

Allgemein

PropertyTemperatureValueConditionRelated StandardsShape

Dichte

2.71 g/cm³

Show Material materials with Dichte of 2.71 g/cm³

H24

EN 573-3, EN 485, EN 541, EN 546, EN 683

20.0 °C

2.71 g/cm³

Show Material materials with Dichte of 2.71 g/cm³

H24

DIN 1725-1, EN 573-3, EN 573-4

Flat

Mechanisch

PropertyTemperatureValueConditionRelated StandardsShapeComment

Dehnung

2.0 %

Show Material materials with Dehnung of 2.0 %

H24

EN 573-3, EN 541, EN 546

A50

3.0 %

Show Material materials with Dehnung of 3.0 %

H24

EN 573-3, EN 485, EN 546

A50

4.0 %

Show Material materials with Dehnung of 4.0 %

H24

EN 573-3, EN 485, EN 546, EN 683

A50

5.0 %

Show Material materials with Dehnung of 5.0 %

H24

EN 573-3, EN 485, EN 546, EN 683

A50

6.0 %

Show Material materials with Dehnung of 6.0 %

H24

EN 573-3, EN 485, EN 683

A50

7.0 %

Show Material materials with Dehnung of 7.0 %

H24

EN 573-3, EN 485

A50

20.0 °C

4.0 %

Show Material materials with Dehnung of 4.0 %

H24

DIN 1725-1, EN 573-3, EN 573-4

Flat

A10

20.0 °C

5.0 %

Show Material materials with Dehnung of 5.0 %

H24

DIN 1725-1, EN 573-3, EN 573-4

Flat

A10

20.0 °C

7.0 %

Show Material materials with Dehnung of 7.0 %

H24

DIN 1725-1, EN 573-3, EN 573-4

Flat

Elastizitätsmodul

70.0 GPa

Show Material materials with Elastizitätsmodul of 70.0 GPa

H24

EN 573-3, EN 485, EN 541, EN 546, EN 683

Härte, Brinell

40.0 [-]

Show Material materials with Härte, Brinell of 40.0 [-]

H24

EN 573-3, EN 485

20.0 °C

40.0 [-]

Show Material materials with Härte, Brinell of 40.0 [-]

H24

DIN 1725-1, EN 573-3, EN 573-4

Flat

Plane-Strain Fracture Toughnes

22.0 - 35.0 MPa·√m

Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m

Typical for Wrought 8000 Series Aluminium

Poissonzahl

0.33 [-]

Show Material materials with Poissonzahl of 0.33 [-]

Typical for Wrought 8000 Series Aluminium

Zugfestigkeit

110.0 - 165.0 MPa

Show Material materials with Zugfestigkeit of 110.0 - 165.0 MPa

H24

EN 573-3, EN 546, EN 683

120.0 - 160.0 MPa

Show Material materials with Zugfestigkeit of 120.0 - 160.0 MPa

H24

EN 573-3, EN 541

125.0 - 165.0 MPa

Show Material materials with Zugfestigkeit of 125.0 - 165.0 MPa

H24

EN 573-3, EN 485

20.0 °C

130.0 - 170.0 MPa

Show Material materials with Zugfestigkeit of 130.0 - 170.0 MPa

H24

DIN 1725-1, EN 573-3, EN 573-4

Flat

Thermisch

PropertyTemperatureValueConditionRelated StandardsShapeComment

Koeffizient der thermischen Ausdehnung

20 °C

2.35e-05 1/K

Show Material materials with Koeffizient der thermischen Ausdehnung of 2.35e-05 1/K

H24

EN 573-3, EN 485, EN 541, EN 546, EN 683

100 °C

2.35e-05 1/K

Show Material materials with Koeffizient der thermischen Ausdehnung of 2.35e-05 1/K

H24

EN 573-3, EN 485, EN 541, EN 546, EN 683

Schmelzpunkt

640.0 - 655.0 °C

Show Material materials with Schmelzpunkt of 640.0 - 655.0 °C

H24

EN 573-3, EN 485, EN 541, EN 546, EN 683

Spezifische Wärmekapazität

920.0 J/(kg·K)

Show Material materials with Spezifische Wärmekapazität of 920.0 J/(kg·K)

Typical for Wrought 8000 Series Aluminium

Wärmeleitfähigkeit

20.0 °C

210.0 - 220.0 W/(m·K)

Show Material materials with Wärmeleitfähigkeit of 210.0 - 220.0 W/(m·K)

H24

DIN 1725-1, EN 573-3, EN 573-4, EN 485, EN 541, EN 546, EN 683

Flat

Elektrisch

PropertyTemperatureValueConditionRelated StandardsShape

Elektrische Leitfähigkeit

20.0 °C

34000000.0 - 35000000.0 S/m

Show Material materials with Elektrische Leitfähigkeit of 34000000.0 - 35000000.0 S/m

H24

DIN 1725-1, EN 573-3, EN 573-4, EN 485, EN 541, EN 546, EN 683

Flat

spezifischer Widerstand

2.86e-08 - 2.94e-08 Ω·m

Show Material materials with spezifischer Widerstand of 2.86e-08 - 2.94e-08 Ω·m

H24

EN 573-3, EN 485, EN 541, EN 546, EN 683

Chemical properties

PropertyValueConditionRelated StandardsShape

Chrom

0.1 %

Show Material materials with Chrom of 0.1 %

H24

EN 573-3, EN 485, EN 541, EN 546, EN 683

Eisen

0.5 - 1.0 %

Show Material materials with Eisen of 0.5 - 1.0 %

H24

DIN 1725-1, EN 573-3, EN 573-4, EN 485, EN 541, EN 546, EN 683

Flat

Kupfer

0.1 %

Show Material materials with Kupfer of 0.1 %

H24

DIN 1725-1, EN 573-3, EN 573-4, EN 485, EN 541, EN 546, EN 683

Flat

Magnesium

0.1 %

Show Material materials with Magnesium of 0.1 %

H24

EN 573-3, EN 485, EN 541, EN 546, EN 683

Mangan

0.1 %

Show Material materials with Mangan of 0.1 %

H24

DIN 1725-1, EN 573-3, EN 573-4, EN 485, EN 541, EN 546, EN 683

Flat

Silizium

0.4 - 0.8 %

Show Material materials with Silizium of 0.4 - 0.8 %

H24

DIN 1725-1, EN 573-3, EN 573-4, EN 485, EN 541, EN 546, EN 683

Flat

Titan

0.05

Show Material materials with Titan of 0.05

H24

DIN 1725-1, EN 573-3, EN 573-4

Flat

Zink

0.1 %

Show Material materials with Zink of 0.1 %

H24

DIN 1725-1, EN 573-3, EN 573-4, EN 485, EN 541, EN 546, EN 683

Flat