Allgemein
Property | Value | Condition | Related Standards |
---|---|---|---|
Dichte | 2.71 g/cm³ Show Material materials with Dichte of 2.71 g/cm³ | H26 | EN 573-3, EN 485, EN 546 |
Mechanisch
Property | Value | Condition | Related Standards | Comment |
---|---|---|---|---|
Elastizitätsmodul | 70.0 GPa Show Material materials with Elastizitätsmodul of 70.0 GPa | H26 | EN 573-3, EN 485, EN 546 | |
Härte, Brinell | 46.0 [-] Show Material materials with Härte, Brinell of 46.0 [-] | H26 | EN 573-3, EN 485 | |
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 8000 Series Aluminium | ||
Poissonzahl | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | Typical for Wrought 8000 Series Aluminium | ||
Zugfestigkeit | 140.0 - 185.0 MPa Show Material materials with Zugfestigkeit of 140.0 - 185.0 MPa | H26 | EN 573-3, EN 546 | |
145.0 - 185.0 MPa Show Material materials with Zugfestigkeit of 145.0 - 185.0 MPa | H26 | EN 573-3, EN 485 |
Thermisch
Property | Temperature | Value | Condition | Related Standards | Comment |
---|---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 20 °C | 2.35e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.35e-05 1/K | H26 | EN 573-3, EN 485, EN 546 | |
100 °C | 2.35e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.35e-05 1/K | H26 | EN 573-3, EN 485, EN 546 | ||
Schmelzpunkt | 640.0 - 655.0 °C Show Material materials with Schmelzpunkt of 640.0 - 655.0 °C | H26 | EN 573-3, EN 485, EN 546 | ||
Spezifische Wärmekapazität | 920.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 920.0 J/(kg·K) | Typical for Wrought 8000 Series Aluminium | |||
Wärmeleitfähigkeit | 210.0 - 220.0 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 210.0 - 220.0 W/(m·K) | H26 | EN 573-3, EN 485, EN 546 |
Elektrisch
Property | Value | Condition | Related Standards |
---|---|---|---|
Elektrische Leitfähigkeit | 34000000.0 - 35000000.0 S/m Show Material materials with Elektrische Leitfähigkeit of 34000000.0 - 35000000.0 S/m | H26 | EN 573-3, EN 485, EN 546 |
spezifischer Widerstand | 2.86e-08 - 2.94e-08 Ω·m Show Material materials with spezifischer Widerstand of 2.86e-08 - 2.94e-08 Ω·m | H26 | EN 573-3, EN 485, EN 546 |
Chemical properties
Property | Value | Condition | Related Standards |
---|---|---|---|
Chrom | 0.1 % Show Material materials with Chrom of 0.1 % | H26 | EN 573-3, EN 485, EN 546 |
Eisen | 0.5 - 1.0 % Show Material materials with Eisen of 0.5 - 1.0 % | H26 | EN 573-3, EN 485, EN 546 |
Kupfer | 0.1 % Show Material materials with Kupfer of 0.1 % | H26 | EN 573-3, EN 485, EN 546 |
Magnesium | 0.1 % Show Material materials with Magnesium of 0.1 % | H26 | EN 573-3, EN 485, EN 546 |
Mangan | 0.1 % Show Material materials with Mangan of 0.1 % | H26 | EN 573-3, EN 485, EN 546 |
Silizium | 0.4 - 0.8 % Show Material materials with Silizium of 0.4 - 0.8 % | H26 | EN 573-3, EN 485, EN 546 |
Zink | 0.1 % Show Material materials with Zink of 0.1 % | H26 | EN 573-3, EN 485, EN 546 |