The alloy is characterised by a good corrosion resistance. It is sea water steady and resistant to saline atmosphere. The Mg content increases the strength, but the cold forming capacity decreases. The material is nature hard, i.e. only by a cold forming and not by a purposeful heat treatment a strength increase can be attained. It is well polishable and anodisable. The splinter-giving machinability becomes better with increasing Mg content, just as the weldability. From the AlMg alloys the mark AlMg1,5 has to exhibit only relatively small mechanical properties. Standardised semi-finished material only for tubes in accordance to DIN 1746 and for extruded profiles according to DIN 1748. Application: Ferrules for wires rope in accordance to DIN 3093. In the civil engineering for carrying constructions, for transport containers. In electro-technology for antennas and parabolic reflectors.

Related Standards

Equivalent Materials

Diese Materialdaten wurden von WIAM,AluKey zur Verfügung gestellt

Alle Daten beziehen sich auf Raumtemperatur soweit nicht anderweitig spezifiziert. SI Einheiten werden verwendt soweit nicht anderweitig spezifiziert.
Äquivalente Standards sind ähnlich zu einem oder mehreren Standards die der Anbieter angegeben hat. Manche äquivalente Standards können strikter sein oder außerhalb der Bedingungen des ursprünglichen Standards.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Eigenschaften

Allgemein

PropertyTemperatureValueConditionRelated StandardsShape

Dichte

2.69 g/cm³

Show Material materials with Dichte of 2.69 g/cm³

H14

EN 573-3, EN 1301

20.0 °C

2.68 g/cm³

Show Material materials with Dichte of 2.68 g/cm³

H14

DIN 1725-1, EN 573-3, EN 573-4

Tube

Mechanisch

PropertyTemperatureValueConditionRelated StandardsShapeComment

Dehnung

4.0 %

Show Material materials with Dehnung of 4.0 %

H14

EN 573-3, EN 1301

20.0 °C

5.0 %

Show Material materials with Dehnung of 5.0 %

H14

DIN 1725-1, EN 573-3, EN 573-4

Tube

A10

20.0 °C

6.0 %

Show Material materials with Dehnung of 6.0 %

H14

DIN 1725-1, EN 573-3, EN 573-4

Tube

Elastizitätsmodul

70.0 GPa

Show Material materials with Elastizitätsmodul of 70.0 GPa

H14

EN 573-3, EN 1301

20.0 °C

65.0 - 70.0 GPa

Show Material materials with Elastizitätsmodul of 65.0 - 70.0 GPa

H14

DIN 1725-1, EN 573-3, EN 573-4

Tube

Härte, Brinell

20.0 °C

45.0 [-]

Show Material materials with Härte, Brinell of 45.0 [-]

H14

DIN 1725-1, EN 573-3, EN 573-4

Tube

Plane-Strain Fracture Toughnes

22.0 - 35.0 MPa·√m

Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m

Typical for Wrought 5000 Series Aluminium

Poissonzahl

0.33 [-]

Show Material materials with Poissonzahl of 0.33 [-]

Typical for Wrought 5000 Series Aluminium

Schubmodule

20.0 °C

26.5 GPa

Show Material materials with Schubmodule of 26.5 GPa

H14

DIN 1725-1, EN 573-3, EN 573-4

Tube

Zugfestigkeit

195.0 - 245.0 MPa

Show Material materials with Zugfestigkeit of 195.0 - 245.0 MPa

H14

EN 573-3, EN 1301

20.0 °C

175.0 MPa

Show Material materials with Zugfestigkeit of 175.0 MPa

H14

DIN 1725-1, EN 573-3, EN 573-4

Tube

Thermisch

PropertyTemperatureValueConditionRelated StandardsShapeComment

Koeffizient der thermischen Ausdehnung

20 °C

2.38e-05 1/K

Show Material materials with Koeffizient der thermischen Ausdehnung of 2.38e-05 1/K

H14

EN 573-3, EN 1301

100 °C

2.38e-05 1/K

Show Material materials with Koeffizient der thermischen Ausdehnung of 2.38e-05 1/K

H14

EN 573-3, EN 1301

Max. Betriebstemperatur

150.0 °C

Show Material materials with Max. Betriebstemperatur of 150.0 °C

Typical for Wrought 5000 Series Aluminium

Schmelzpunkt

560.0 - 655.0 °C

Show Material materials with Schmelzpunkt of 560.0 - 655.0 °C

Typical for Wrought 5000 Series Aluminium

Spezifische Wärmekapazität

20.0 °C

921.0 J/(kg·K)

Show Material materials with Spezifische Wärmekapazität of 921.0 J/(kg·K)

H14

DIN 1725-1, EN 573-3, EN 573-4

Tube

Wärmeleitfähigkeit

20.0 °C

135.0 - 167.0 W/(m·K)

Show Material materials with Wärmeleitfähigkeit of 135.0 - 167.0 W/(m·K)

H14

DIN 1725-1, EN 573-3, EN 573-4

Tube

Elektrisch

PropertyTemperatureValueConditionRelated StandardsShapeComment

Elektrische Leitfähigkeit

20.0 °C

22000000.0 - 26000000.0 S/m

Show Material materials with Elektrische Leitfähigkeit of 22000000.0 - 26000000.0 S/m

H14

DIN 1725-1, EN 573-3, EN 573-4

Tube

spezifischer Widerstand

3.3e-08 - 5e-08 Ω·m

Show Material materials with spezifischer Widerstand of 3.3e-08 - 5e-08 Ω·m

Typical for Wrought 5000 Series Aluminium

Chemical properties

PropertyValueConditionRelated StandardsShape

Chrom

0.3 %

Show Material materials with Chrom of 0.3 %

H14

DIN 1725-1, EN 573-3, EN 573-4, EN 1301

Tube

Eisen

0.45 %

Show Material materials with Eisen of 0.45 %

H14

DIN 1725-1, EN 573-3, EN 573-4

Tube

0.45 %

Show Material materials with Eisen of 0.45 %

H14

EN 573-3, EN 1301

Kupfer

0.05 %

Show Material materials with Kupfer of 0.05 %

H14

DIN 1725-1, EN 573-3, EN 573-4, EN 1301

Tube

Magnesium

1.4 - 2.1 %

Show Material materials with Magnesium of 1.4 - 2.1 %

H14

DIN 1725-1, EN 573-3, EN 573-4, EN 1301

Tube

Mangan

0.25 %

Show Material materials with Mangan of 0.25 %

H14

DIN 1725-1, EN 573-3, EN 573-4, EN 1301

Tube

Silizium

0.3 %

Show Material materials with Silizium of 0.3 %

H14

DIN 1725-1, EN 573-3, EN 573-4, EN 1301

Tube

Titan

0.1 %

Show Material materials with Titan of 0.1 %

H14

DIN 1725-1, EN 573-3, EN 573-4, EN 1301

Tube

Zink

0.2 %

Show Material materials with Zink of 0.2 %

H14

DIN 1725-1, EN 573-3, EN 573-4, EN 1301

Tube

Technological properties

Property
Workability

Good workability.