Description

Pure aluminium This material is well anodically oxidizable, and possesses a good electrical and thermal conductivity. The splinter-giving workability is bad because of danger of smearing. Its mechanical strength is low, the plasticity high. The forming capacity and the chemical as well as the weather proofness are excellent. The material is well suitable for welding and braze welding. Application: Apparatus engineering, roll bond, z-bond, household devices, camp and transportation containers for the chemical, pharmaceutical and food industry, roofing, linings, arts and crafts, packing, flow pressed parts (tubes, tube, doses, bottles), pressure tanks according to AD-W 6/1

Related Standards

Equivalent Materials

Diese Materialdaten wurden von WIAM,AluKey zur Verfügung gestellt

Alle Daten beziehen sich auf Raumtemperatur soweit nicht anderweitig spezifiziert. SI Einheiten werden verwendt soweit nicht anderweitig spezifiziert.
Äquivalente Standards sind ähnlich zu einem oder mehreren Standards die der Anbieter angegeben hat. Manche äquivalente Standards können strikter sein oder außerhalb der Bedingungen des ursprünglichen Standards.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Eigenschaften

Allgemein

PropertyTemperatureValueConditionRelated StandardsShape

Dichte

2.7 g/cm³

Show Material materials with Dichte of 2.7 g/cm³

H18

EN 573-3, EN 1301, EN 485

20.0 °C

2.7 g/cm³

Show Material materials with Dichte of 2.7 g/cm³

H18

DIN 1712-3, EN 573-3, EN 573-4

Sheet, Strip

Mechanisch

PropertyTemperatureValueConditionRelated StandardsShapeComment

Biegewinkel 90°

1.0 °/t

Show Material materials with Biegewinkel 90° of 1.0 °/t

H18

EN 573-3, EN 485

2.0 °/t

Show Material materials with Biegewinkel 90° of 2.0 °/t

H18

EN 573-3, EN 485

2.5 °/t

Show Material materials with Biegewinkel 90° of 2.5 °/t

H18

EN 573-3, EN 485

Dehnung

2.0 %

Show Material materials with Dehnung of 2.0 %

H18

EN 573-3, EN 485

A50

3.0 %

Show Material materials with Dehnung of 3.0 %

H18

EN 573-3, EN 1301

20.0 °C

3.0 %

Show Material materials with Dehnung of 3.0 %

H18

DIN 1712-3, EN 573-3, EN 573-4

Sheet, Strip

A10

20.0 °C

4.0 %

Show Material materials with Dehnung of 4.0 %

H18

DIN 1712-3, EN 573-3, EN 573-4

Sheet, Strip

Elastizitätsmodul

70.0 GPa

Show Material materials with Elastizitätsmodul of 70.0 GPa

H18

EN 573-3, EN 1301, EN 485

20.0 °C

60.0 - 70.0 GPa

Show Material materials with Elastizitätsmodul of 60.0 - 70.0 GPa

H18

DIN 1712-3, EN 573-3, EN 573-4

Sheet, Strip

Härte, Brinell

40.0 [-]

Show Material materials with Härte, Brinell of 40.0 [-]

H18

EN 573-3, EN 485

20.0 °C

36.0 [-]

Show Material materials with Härte, Brinell of 36.0 [-]

H18

DIN 1712-3, EN 573-3, EN 573-4

Sheet, Strip

Plane-Strain Fracture Toughnes

22.0 - 35.0 MPa·√m

Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m

Typical for Wrought 1000 Series Aluminium

Poissonzahl

0.33 [-]

Show Material materials with Poissonzahl of 0.33 [-]

Typical for Wrought 1000 Series Aluminium

Schubmodule

20.0 °C

25.0 - 26.5 GPa

Show Material materials with Schubmodule of 25.0 - 26.5 GPa

H18

DIN 1712-3, EN 573-3, EN 573-4

Sheet, Strip

Zugfestigkeit

125.0 MPa

Show Material materials with Zugfestigkeit of 125.0 MPa

H18

EN 573-3, EN 1301, EN 485

20.0 °C

120.0 - 160.0 MPa

Show Material materials with Zugfestigkeit of 120.0 - 160.0 MPa

H18

DIN 1712-3, EN 573-3, EN 573-4

Sheet, Strip

Thermisch

PropertyTemperatureValueConditionRelated StandardsShape

Koeffizient der thermischen Ausdehnung

20 °C

2.35e-05 1/K

Show Material materials with Koeffizient der thermischen Ausdehnung of 2.35e-05 1/K

H18

EN 573-3, EN 1301, EN 485

100 °C

2.35e-05 1/K

Show Material materials with Koeffizient der thermischen Ausdehnung of 2.35e-05 1/K

H18

EN 573-3, EN 1301, EN 485

Schmelzpunkt

659.0 °C

Show Material materials with Schmelzpunkt of 659.0 °C

H18

EN 573-3, EN 1301, EN 485

Spezifische Wärmekapazität

20.0 °C

921.0 J/(kg·K)

Show Material materials with Spezifische Wärmekapazität of 921.0 J/(kg·K)

H18

DIN 1712-3, EN 573-3, EN 573-4

Sheet, Strip

Wärmeleitfähigkeit

225 W/(m·K)

Show Material materials with Wärmeleitfähigkeit of 225 W/(m·K)

H18

EN 573-3, EN 1301, EN 485

20.0 °C

215.0 W/(m·K)

Show Material materials with Wärmeleitfähigkeit of 215.0 W/(m·K)

H18

DIN 1712-3, EN 573-3, EN 573-4

Sheet, Strip

Elektrisch

PropertyTemperatureValueConditionRelated StandardsShape

Elektrische Leitfähigkeit

34500000.0 - 35000000.0 S/m

Show Material materials with Elektrische Leitfähigkeit of 34500000.0 - 35000000.0 S/m

H18

EN 573-3, EN 1301, EN 485

20.0 °C

35800000.0 - 36800000.0 S/m

Show Material materials with Elektrische Leitfähigkeit of 35800000.0 - 36800000.0 S/m

H18

DIN 1712-3, EN 573-3, EN 573-4

Sheet, Strip

spezifischer Widerstand

2.86e-08 - 2.9e-08 Ω·m

Show Material materials with spezifischer Widerstand of 2.86e-08 - 2.9e-08 Ω·m

H18

EN 573-3, EN 1301, EN 485

Chemical properties

PropertyValueConditionRelated StandardsShape

Aluminium

99.7 %

Show Material materials with Aluminium of 99.7 %

H18

EN 573-3, EN 1301, EN 485

Eisen

0.25 %

Show Material materials with Eisen of 0.25 %

H18

DIN 1712-3, EN 573-3, EN 573-4

Sheet, Strip

0.25 %

Show Material materials with Eisen of 0.25 %

H18

EN 573-3, EN 1301, EN 485

Kupfer

0.03 %

Show Material materials with Kupfer of 0.03 %

H18

DIN 1712-3, EN 573-3, EN 573-4, EN 1301, EN 485

Sheet, Strip

Magnesium

0.03 %

Show Material materials with Magnesium of 0.03 %

H18

DIN 1712-3, EN 573-3, EN 573-4, EN 1301, EN 485

Sheet, Strip

Mangan

0.03 %

Show Material materials with Mangan of 0.03 %

H18

DIN 1712-3, EN 573-3, EN 573-4, EN 1301, EN 485

Sheet, Strip

Silizium

0.2 %

Show Material materials with Silizium of 0.2 %

H18

DIN 1712-3, EN 573-3, EN 573-4, EN 1301, EN 485

Sheet, Strip

Titan

0.03 %

Show Material materials with Titan of 0.03 %

H18

DIN 1712-3, EN 573-3, EN 573-4, EN 1301, EN 485

Sheet, Strip

Zink

0.07 %

Show Material materials with Zink of 0.07 %

H18

DIN 1712-3, EN 573-3, EN 573-4, EN 1301, EN 485

Sheet, Strip

Technological properties

Property
Anodizing

decorative: very good, Protective: very good

Brazing

hard brazing (with flux/ without flux): very good / very good, friction soldering: very good, soft brazing with flux: very good

Workability

Bending / Spinning (cold): very good / very good, Impact extrusion (cold): very good, Deep drawing / upsetting (Condition) very good (H14) / very good (H12)