Allgemein
Property | Value | Condition | Related Standards |
---|---|---|---|
Dichte | 2.7 g/cm³ Show Material materials with Dichte of 2.7 g/cm³ | H111 | EN 573-3, EN 485, EN 755 |
Mechanisch
Property | Value | Condition | Related Standards | Comment |
---|---|---|---|---|
Elastizitätsmodul | 70.0 GPa Show Material materials with Elastizitätsmodul of 70.0 GPa | H111 | EN 573-3, EN 485, EN 755 | |
Härte, Brinell | 20.0 [-] Show Material materials with Härte, Brinell of 20.0 [-] | H111 | EN 573-3, EN 485, EN 755 | |
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 1000 Series Aluminium | ||
Poissonzahl | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | Typical for Wrought 1000 Series Aluminium | ||
Schubmodule | 25.9 GPa Show Material materials with Schubmodule of 25.9 GPa | Typical for Wrought 1000 Series Aluminium | ||
Zugfestigkeit | 60.0 MPa Show Material materials with Zugfestigkeit of 60.0 MPa | H111 | EN 573-3, EN 755 | |
65.0 - 105.0 MPa Show Material materials with Zugfestigkeit of 65.0 - 105.0 MPa | H111 | EN 573-3, EN 485 |
Thermisch
Property | Temperature | Value | Condition | Related Standards | Comment |
---|---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 20 °C | 2.35e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.35e-05 1/K | H111 | EN 573-3, EN 485, EN 755 | |
100 °C | 2.35e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.35e-05 1/K | H111 | EN 573-3, EN 485, EN 755 | ||
Schmelzpunkt | 658.0 °C Show Material materials with Schmelzpunkt of 658.0 °C | H111 | EN 573-3, EN 485, EN 755 | ||
Spezifische Wärmekapazität | 900.0 - 963.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 900.0 - 963.0 J/(kg·K) | Typical for Wrought 1000 Series Aluminium | |||
Wärmeleitfähigkeit | 230 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 230 W/(m·K) | H111 | EN 573-3, EN 485, EN 755 |
Elektrisch
Property | Value | Condition | Related Standards |
---|---|---|---|
Elektrische Leitfähigkeit | 34500000.0 - 35500000.0 S/m Show Material materials with Elektrische Leitfähigkeit of 34500000.0 - 35500000.0 S/m | H111 | EN 573-3, EN 485, EN 755 |
spezifischer Widerstand | 2.82e-08 - 2.9e-08 Ω·m Show Material materials with spezifischer Widerstand of 2.82e-08 - 2.9e-08 Ω·m | H111 | EN 573-3, EN 485, EN 755 |
Chemical properties
Property | Value | Condition | Related Standards |
---|---|---|---|
Aluminium | 99.5 % Show Material materials with Aluminium of 99.5 % | H111 | EN 573-3, EN 485, EN 755 |
Eisen | 0.40 % Show Material materials with Eisen of 0.40 % | H111 | EN 573-3, EN 485, EN 755 |
Kupfer | 0.02 % Show Material materials with Kupfer of 0.02 % | H111 | EN 573-3, EN 485, EN 755 |
Magnesium | 0.05 % Show Material materials with Magnesium of 0.05 % | H111 | EN 573-3, EN 485, EN 755 |
Silizium | 0.25 % Show Material materials with Silizium of 0.25 % | H111 | EN 573-3, EN 485, EN 755 |
Zink | 0.05 % Show Material materials with Zink of 0.05 % | H111 | EN 573-3, EN 485, EN 755 |
Technological properties
Property | ||
---|---|---|
Brazing | Excellent | |
Workability | Excellent workability. |