Chemical properties
Property | Value |
---|---|
Aluminium | 0.01 % Show Material materials with Aluminium of 0.01 % |
Andere | Rest Zn |
Blei | 0.05 % Show Material materials with Blei of 0.05 % |
Eisen | 0.25 - 1.25 % Show Material materials with Eisen of 0.25 - 1.25 % |
Kupfer | 56 - 60 % Show Material materials with Kupfer of 56 - 60 % |
Mangan | 0.01 - 0.5 % Show Material materials with Mangan of 0.01 - 0.5 % |
Silizium | 0.04 - 0.15 % Show Material materials with Silizium of 0.04 - 0.15 % |
Zinn | 0.75 - 1.1 % Show Material materials with Zinn of 0.75 - 1.1 % |