Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 8.4 g/cm³ Show Material materials with Dichte of 8.4 g/cm³ |
Thermisch
Property | Temperature | Value |
---|---|---|
Schmelzpunkt | 890 - 910 °C Show Material materials with Schmelzpunkt of 890 - 910 °C | |
Wärmeleitfähigkeit | 23.0 °C | 120 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 120 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 23.0 °C | 1.50E+7 S/m Show Material materials with Elektrische Leitfähigkeit of 1.50E+7 S/m |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.01 % Show Material materials with Aluminium of 0.01 % |
Andere | Rest Zn, total 0.2 |
Blei | 0.03 % Show Material materials with Blei of 0.03 % |
Eisen | 0.2 % Show Material materials with Eisen of 0.2 % |
Kupfer | 58 - 62 % Show Material materials with Kupfer of 58 - 62 % |
Mangan | 0.3 % Show Material materials with Mangan of 0.3 % |
Silizium | 0.1 - 0.5 % Show Material materials with Silizium of 0.1 - 0.5 % |
Zinn | 1 % Show Material materials with Zinn of 1 % |