Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 8.7 g/cm³ Show Material materials with Dichte of 8.7 g/cm³ |
Thermisch
Property | Temperature | Value |
---|---|---|
Schmelzpunkt | 1100 - 1145 °C Show Material materials with Schmelzpunkt of 1100 - 1145 °C | |
Wärmeleitfähigkeit | 23.0 °C | 45 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 45 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 23.0 °C | 4.00E+6 - 5.00E+6 S/m Show Material materials with Elektrische Leitfähigkeit of 4.00E+6 - 5.00E+6 S/m |
Chemical properties
Property | Value |
---|---|
Andere | Rest Cu, total 0.5 |
Blei | 0.02 % Show Material materials with Blei of 0.02 % |
Eisen | 2.5 % Show Material materials with Eisen of 2.5 % |
Kohlenstoff | 0.05 % Show Material materials with Kohlenstoff of 0.05 % |
Mangan | 0.5 - 2 % Show Material materials with Mangan of 0.5 - 2 % |
Nickel | 9 - 11 % Show Material materials with Nickel of 9 - 11 % |
Phosphor | 0.02 % Show Material materials with Phosphor of 0.02 % |
Schwefel | 0.015 % Show Material materials with Schwefel of 0.015 % |
Silizium | 0.5 % Show Material materials with Silizium of 0.5 % |
Titan | 0.5 % Show Material materials with Titan of 0.5 % |