Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 7.7 g/cm³ Show Material materials with Dichte of 7.7 g/cm³ |
Thermisch
Property | Temperature | Value |
---|---|---|
Schmelzpunkt | 1030 - 1040 °C Show Material materials with Schmelzpunkt of 1030 - 1040 °C | |
Wärmeleitfähigkeit | 23.0 °C | 65 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 65 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 23.0 °C | 8.00E+6 S/m Show Material materials with Elektrische Leitfähigkeit of 8.00E+6 S/m |
Chemical properties
Property | Value |
---|---|
Aluminium | 7.5 - 9.5 % Show Material materials with Aluminium of 7.5 - 9.5 % |
Andere | Rest Cu, total 0.4 |
Blei | 0.02 % Show Material materials with Blei of 0.02 % |
Eisen | 0.5 % Show Material materials with Eisen of 0.5 % |
Mangan | 1 % Show Material materials with Mangan of 1 % |
Nickel | 0.8 % Show Material materials with Nickel of 0.8 % |
Silizium | 0.2 % Show Material materials with Silizium of 0.2 % |
Zink | 0.2 % Show Material materials with Zink of 0.2 % |