Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 7.5 g/cm³ Show Material materials with Dichte of 7.5 g/cm³ |
Thermisch
Property | Temperature | Value |
---|---|---|
Schmelzpunkt | 1015 - 1045 °C Show Material materials with Schmelzpunkt of 1015 - 1045 °C | |
Wärmeleitfähigkeit | 23.0 °C | 35 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 35 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 23.0 °C | 4.00E+6 S/m Show Material materials with Elektrische Leitfähigkeit of 4.00E+6 S/m |
Chemical properties
Property | Value |
---|---|
Aluminium | 8.5 - 9.5 % Show Material materials with Aluminium of 8.5 - 9.5 % |
Andere | Rest Cu, total 0.4 |
Blei | 0.02 % Show Material materials with Blei of 0.02 % |
Eisen | 3 - 4 % Show Material materials with Eisen of 3 - 4 % |
Mangan | 1 - 2 % Show Material materials with Mangan of 1 - 2 % |
Nickel | 4 - 6 % Show Material materials with Nickel of 4 - 6 % |
Silizium | 0.2 % Show Material materials with Silizium of 0.2 % |
Zink | 0.1 % Show Material materials with Zink of 0.1 % |