Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 7.7 g/cm³ Show Material materials with Dichte of 7.7 g/cm³ |
Thermisch
Property | Temperature | Value |
---|---|---|
Schmelzpunkt | 1020 - 1050 °C Show Material materials with Schmelzpunkt of 1020 - 1050 °C | |
Wärmeleitfähigkeit | 23.0 °C | 70 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 70 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 23.0 °C | 6.00E+6 S/m Show Material materials with Elektrische Leitfähigkeit of 6.00E+6 S/m |
Chemical properties
Property | Value |
---|---|
Aluminium | 6.5 - 8.5 % Show Material materials with Aluminium of 6.5 - 8.5 % |
Andere | Rest Cu, total 0.5 |
Blei | 0.02 % Show Material materials with Blei of 0.02 % |
Eisen | 1 % Show Material materials with Eisen of 1 % |
Mangan | 2 % Show Material materials with Mangan of 2 % |
Nickel | 0.8 % Show Material materials with Nickel of 0.8 % |
Silizium | 0.7 % Show Material materials with Silizium of 0.7 % |