Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 7.5 g/cm³ Show Material materials with Dichte of 7.5 g/cm³ |
Thermisch
Property | Temperature | Value |
---|---|---|
Schmelzpunkt | 1030 - 1050 °C Show Material materials with Schmelzpunkt of 1030 - 1050 °C | |
Wärmeleitfähigkeit | 23.0 °C | 30 - 50 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 30 - 50 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 23.0 °C | 5.00E+6 S/m Show Material materials with Elektrische Leitfähigkeit of 5.00E+6 S/m |
Chemical properties
Property | Value |
---|---|
Aluminium | 6.5 - 8.5 % Show Material materials with Aluminium of 6.5 - 8.5 % |
Andere | Rest Cu, total 0.5 |
Blei | 0.02 % Show Material materials with Blei of 0.02 % |
Eisen | 1.5 - 2.5 % Show Material materials with Eisen of 1.5 - 2.5 % |
Mangan | 1.5 - 3 % Show Material materials with Mangan of 1.5 - 3 % |
Nickel | 1.8 - 3 % Show Material materials with Nickel of 1.8 - 3 % |
Silizium | 0.7 % Show Material materials with Silizium of 0.7 % |