Chemical properties
Property | Value |
---|---|
Aluminium | 7.3 - 8.8 % Show Material materials with Aluminium of 7.3 - 8.8 % |
Andere | total 0.4 |
Blei | 0.05 % Show Material materials with Blei of 0.05 % |
Eisen | 0.6 % Show Material materials with Eisen of 0.6 % |
Kupfer | 82 - 84.5 % Show Material materials with Kupfer of 82 - 84.5 % |
Magnesium | 0.04 % Show Material materials with Magnesium of 0.04 % |
Mangan | 5.3 - 6.5 % Show Material materials with Mangan of 5.3 - 6.5 % |
Nickel | 1.2 - 1.8 % Show Material materials with Nickel of 1.2 - 1.8 % |
Silizium | 0.05 % Show Material materials with Silizium of 0.05 % |
Zink | 0.15 % Show Material materials with Zink of 0.15 % |
Zinn | 0.1 % Show Material materials with Zinn of 0.1 % |